Custom 450 plate (UNS S45000, XM-25) is a martensitic precipitation-hardening stainless steel that offers a combination of good corrosion resistance, high strength, excellent toughness, and favorable machinability. Through an aging treatment, the material achieves higher strength while retaining a℃of ductility and toughness. Its corrosion resistance is comparable to that of 304 stainless steel, while its strength level exceeds that of conventional austenitic stainless steels in the annealed condition, making it well-suited for industrial components that require both structural strength and corrosion resistance.
Custom 450 is available in the form of cold-rolled sheets, hot-rolled plates, and precision strip. It is typically supplied in the solution-annealed condition (Condition A)-with a hardness of approximately HRC 28 (<= 285 HB)-which facilitates cold forming, stamping, and machining. Users can apply a single-stage aging treatment to achieve the desired target strength.
| <= 0.05% | |
| <= 1.00% | |
| <= 0.03% | |
| <= 0.03% | |
| <= 1.00% | |
| 14.00 - 16.00% | |
| 5.00 - 7.00% | |
| 0.50 - 1.00% | |
| 1.25 - 1.75% | |
| H900 status(Aging at 480℃) | ||
| >= 860 MPa | >= 1380 MPa | |
| Yield Strength (0.2%) | >= 690 MPa | >= 1240 MPa |
| >=10% | >=10% | |
| HRC 20-28 | HRC 40-46 |
Custom 450 is a martensitic precipitation-hardening stainless steel. Its resistance to intergranular corrosion is primarily determined by its chromium content, heat-treatment condition, and the nature of any precipitates formed at the grain boundaries. Intergranular corrosion testing is used to evaluate whether a material is susceptible to preferential corrosion at the grain boundaries when exposed to specific corrosive media; it also serves as an indicator of the material's microstructural stability and overall corrosion resistance.
Testing Standards: As a martensitic precipitation-hardening stainless steel, Custom 450 can be evaluated for intergranular corrosion resistance using methods such as Practice E of the ASTM A262 standard. The testing process typically involves specimen preparation, exposure to a corrosive medium, and subsequent metallographic examination. The material's resistance to intergranular corrosion is assessed by inspecting the grain boundaries for signs of significant corrosion or cracking.
It should be noted that the scope of ASTM A262 primarily covers austenitic stainless steels. When applied to martensitic precipitation-hardening stainless steels such as Custom 450, the standard is used as a reference, and the test results are evaluated by taking into account the material's actual heat-treatment condition (i.e., solution-annealed or aged).